TECHNET Archives

December 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Tue, 1 Dec 2015 18:37:29 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Agreed. There was no redundancy here, nor was there an effective default condition.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ahne Oosterhof
Sent: Tuesday, December 01, 2015 11:35 AM
To: [log in to unmask]
Subject: Re: [TN] Airbus crash pinned (in part) on solder joint failures

Figure 35: Electronic Module of RTLU

Not much of a failure to cause the loss of life and an aircraft!

Conclusion: End-use of a board module dictates extreme level of attention to design and testing protocols.

Ahne.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Buetow
Sent: Tuesday, December 1, 2015 6:28 AM
To: [log in to unmask]
Subject: [TN] Airbus crash pinned (in part) on solder joint failures

Here's the report: http://kemhubri.dephub.go.id/knkt/ntsc_home/ntsc.htm



Discussion of the electrical short and cracked solder joint begins on page 104.





Best,



Mike



Mike Buetow

PCD&F/Circuits Assembly

w/m: 617-327-4702

@mikebuetow



The 2015 CIRCUITS ASSEMBLY *Directory of EMS Companies:* circuitsassembly.com/dems


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2