TECHNET Archives

December 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Tue, 1 Dec 2015 11:13:18 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Gregg Owens <[log in to unmask]>
Message-ID:
Subject:
From:
Gregg Owens <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Who says engineers don't have a sense of humor! LOL

Gregg

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, December 01, 2015 11:05 AM
To: [log in to unmask]
Subject: Re: [TN] Airbus crash pinned (in part) on solder joint failures

I had not thought of that, you are quite right to point that out. So, I did an advanced image search using the exact same color and texture of the rusty orange substance taken from the article and figured out what it was.
https://en.wikipedia.org/wiki/Patrick_Star


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of MacFadden, Todd
Sent: Tuesday, December 01, 2015 12:06 PM
To: [log in to unmask]
Subject: Re: [TN] Airbus crash pinned (in part) on solder joint failures

The rusty orange appearance is likely explained by this: 

" The RTLU which was recovered from the accident site..."

i.e., the ocean.



Todd


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Garcia, Rigo (GSFC-370.0)[ARES CORP]
Sent: Tuesday, December 1, 2015 12:54 PM
To: [log in to unmask]
Subject: Re: [TN] Airbus crash pinned (in part) on solder joint failures

Curious of what everybody thinks.

Looking at Figure 35 on page 66 of the report...

1. Does it look like a typical solder joint?
2. Why the rusty orangey appearance on the area surrounding the solder joint?

Rigo Garcia

“The future belongs to those who believe in the beauty of their dreams” – Eleanor Roosevelt 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Watson, Howard August
Sent: Tuesday, December 01, 2015 11:30 AM
To: [log in to unmask]
Subject: Re: [TN] Airbus crash pinned (in part) on solder joint failures

Mike,

Thanks for sending this link - that report was very interesting. Note that the detailed discussion of solder cracks along with interesting photos is also on page 66. 

Thanks,

Howard  Watson 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Buetow
Sent: Tuesday, December 01, 2015 7:28 AM
To: [log in to unmask]
Subject: [TN] Airbus crash pinned (in part) on solder joint failures

Here's the report: http://kemhubri.dephub.go.id/knkt/ntsc_home/ntsc.htm



Discussion of the electrical short and cracked solder joint begins on page 104.





Best,



Mike



Mike Buetow

PCD&F/Circuits Assembly

w/m: 617-327-4702

@mikebuetow



The 2015 CIRCUITS ASSEMBLY *Directory of EMS Companies:* circuitsassembly.com/dems


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2