I'm not worried about that particular one. There are 3 major in the spectrum, even though there are overlappings and not just with Ca
Vladimir
---- On Thu, 10 Dec 2015 06:01:11 -0800 Bhanu Sood<[log in to unmask]> wrote ----
> Not sure why a Sn label appears at 0.3keV??
>
> As you know, there exist more than a few peak overlaps and Sn-Ca is
> classic, fyi.. CaKα 3.7keV, CaLα0.3, SnLα 3.4
>
> I recommend a rescan point and ID, much higher mag, and increase your
> accelerating voltage so you can look at binding energies in 10keV+ range..
>
> Bhanu
>
>
>
> On Wed, Dec 9, 2015 at 7:55 PM, Vladimir Igoshev <[log in to unmask]
> > wrote:
>
> > No underfill or any other fancy stuff
> >
> > ---- On Wed, 09 Dec 2015 16:53:28 -0800 Yuan-chia Joyce Koo<
> > [log in to unmask]> wrote ----
> > > tin oxalyate used for epoxy catalyst... there were works for flux/
> > > underfill one step stuff utilize flux by product as catalyst for
> > > curing... (can't remember which group did that...)
> > > jk
> > > On Dec 9, 2015, at 7:03 PM, Vladimir Igoshev wrote:
> > >
> > > > Hi Dave,
> > > >
> > > > Not really. It doesn't "burn" or "curl" much under the beam, so
> > > > it's solid.
> > > >
> > > > Vladimir
> > > >
> > > > ---- On Wed, 09 Dec 2015 15:51:29 -0800 David
> > > > Hillman<[log in to unmask]> wrote ----
> > > >> Thank you Steve!
> > > >>
> > > >> Vlad - does the substance slightly charge in the SEM?
> > > >>
> > > >> Dave
> > > >>
> > > >> On Wed, Dec 9, 2015 at 5:46 PM, Steve Gregory <[log in to unmask]>
> > > >> wrote:
> > > >>
> > > >>> Hi Dave and Vlad,
> > > >>>
> > > >>> I have it up here:
> > > >>>
> > > >>> http://stevezeva.homestead.com/What_else_it_can_be.pdf
> > > >>>
> > > >>> Steve
> > > >>>
> > > >>> On Wed, Dec 9, 2015 at 4:34 PM, David Hillman <
> > > >>> [log in to unmask]> wrote:
> > > >>>
> > > >>>> HI Vlad - we can't open Dropbox here due to firewall
> > > >>>> restrictions so can
> > > >>>> you have Steve G. post the pictures?
> > > >>>>
> > > >>>> Dave Hillman
> > > >>>> Rockwell Collins
> > > >>>> [log in to unmask]
> > > >>>>
> > > >>>> On Wed, Dec 9, 2015 at 4:59 PM, Vladimir Igoshev <
> > > >>>> [log in to unmask]
> > > >>>>> wrote:
> > > >>>>
> > > >>>>> HI everyone,
> > > >>>>>
> > > >>>>> I'm attaching a link to a file showing something I'd appreciate
> > > >>>>> your
> > > >>>>> thoughts on. It's a cross-section of a QFN on an IAg board;
> > > >>>>> Pb-free/no-clean process. As you can see from the EDS spectrum,
> > > >>>>> that
> > > >>>>> greyish stuff between pins has pretty much only Sn and O in its
> > > >>>> elemental
> > > >>>>> composition.
> > > >>>>>
> > > >>>>> I know there is burn flux residue around solder joints but that
> > > >>>>> stuff
> > > >>>>> doesn't have any C in it. The question I have is what is it.
> > > >>>>>
> > > >>>>> I spoke to Bev and both of us are still puzzled.
> > > >>>>>
> > > >>>>> Here is the link:
> > > >>>>>
> > > >>>> https://www.dropbox.com/s/3wbj62vqjyhvj2y/What%20else%20it%20can%
> > > >>>> 20be.pdf?dl=0
> > > >>>>>
> > > >>>>> Thank you very much in advance.
> > > >>>>>
> > > >>>>> Regards,
> > > >>>>>
> > > >>>>> Vladimir
> > > >>>>>
> > > >>>>> SENTEC
> > > >>>>>
> > > >>>>>
> > > >>>>> __________________________________________________________________
> > > >>>>> ____
> > > >>>>> This email has been scanned by the Symantec Email Security.cloud
> > > >>>> service.
> > > >>>>> For more information please contact helpdesk at x2960 or
> > > >>>> [log in to unmask]
> > > >>>>> __________________________________________________________________
> > > >>>>> ____
> > > >>>>>
> > > >>>>
> > > >>>>
> > > >>>> ___________________________________________________________________
> > > >>>> ___
> > > >>>> This email has been scanned by the Symantec Email Security.cloud
> > > >>>> service.
> > > >>>> For more information please contact helpdesk at x2960 or
> > > >>>> [log in to unmask]
> > > >>>> ___________________________________________________________________
> > > >>>> ___
> > > >>>>
> > > >>>
> > > >>>
> > > >>>
> > > >>> This email and any attachments are only for use by the intended
> > > >>> recipient(s) and may contain legally privileged, confidential,
> > > >>> proprietary
> > > >>> or otherwise private information. Any unauthorized use,
> > > >>> reproduction,
> > > >>> dissemination, distribution or other disclosure of the contents
> > > >>> of this
> > > >>> e-mail or its attachments is strictly prohibited. If you have
> > > >>> received this
> > > >>> email in error, please notify the sender immediately and delete the
> > > >>> original.
> > > >>>
> > > >>
> > > >>
> > > >> _____________________________________________________________________
> > > >> _
> > > >> This email has been scanned by the Symantec Email Security.cloud
> > > >> service.
> > > >> For more information please contact helpdesk at x2960 or
> > > >> [log in to unmask]
> > > >> _____________________________________________________________________
> > > >> _
> > > >>
> > > >
> > > >
> > > >
> > > > ______________________________________________________________________
> > > > This email has been scanned by the Symantec Email Security.cloud
> > > > service.
> > > > For more information please contact helpdesk at x2960 or
> > > > [log in to unmask]
> > > > ______________________________________________________________________
> > >
> > >
> > > ______________________________________________________________________
> > > This email has been scanned by the Symantec Email Security.cloud
> > service.
> > > For more information please contact helpdesk at x2960 or
> > [log in to unmask]
> > > ______________________________________________________________________
> > >
> >
> >
> >
> > ______________________________________________________________________
> > This email has been scanned by the Symantec Email Security.cloud service.
> > For more information please contact helpdesk at x2960 or [log in to unmask]
> > ______________________________________________________________________
> >
>
>
>
> --
> Bhanu Sood
> Tel: (202) 468-8449
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|