dip flux works well (you might want to get low solid or low residue flux)
if you have good pick and place machine and good reflow profile... at
least it used to work well...
jk
> Dear Technetters:
>
> In reviewing the IPC 7095 BGA guidelines I noticed a mention of liquid
> based fluxes for BGA rework. Has anyone heard of liquid fluxes being
> robust
> enough for Sn63 or lead-free rework processes?
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
> --
> Thanks
>
> Bob Wettermann/BEST
>