TECHNET Archives

December 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Garcia, Rigo (GSFC-370.0)[ARES CORP]" <[log in to unmask]>
Date:
Tue, 1 Dec 2015 12:06:09 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Message-ID:
Subject:
From:
David Hillman <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=UTF-8
MIME-Version:
1.0
Parts/Attachments:
text/plain (100 lines)
Hi Rigo - based on the report, the electronics were exposed to sea water so
visual observations are going to be confounded.

Dave Hillman
Rockwell Collins
[log in to unmask]

On Tue, Dec 1, 2015 at 11:53 AM, Garcia, Rigo (GSFC-370.0)[ARES CORP] <
[log in to unmask]> wrote:

> Curious of what everybody thinks.
>
> Looking at Figure 35 on page 66 of the report...
>
> 1. Does it look like a typical solder joint?
> 2. Why the rusty orangey appearance on the area surrounding the solder
> joint?
>
> Rigo Garcia
>
> “The future belongs to those who believe in the beauty of their dreams” –
> Eleanor Roosevelt
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Watson, Howard August
> Sent: Tuesday, December 01, 2015 11:30 AM
> To: [log in to unmask]
> Subject: Re: [TN] Airbus crash pinned (in part) on solder joint failures
>
> Mike,
>
> Thanks for sending this link - that report was very interesting. Note that
> the detailed discussion of solder cracks along with interesting photos is
> also on page 66.
>
> Thanks,
>
> Howard  Watson
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Buetow
> Sent: Tuesday, December 01, 2015 7:28 AM
> To: [log in to unmask]
> Subject: [TN] Airbus crash pinned (in part) on solder joint failures
>
> Here's the report: http://kemhubri.dephub.go.id/knkt/ntsc_home/ntsc.htm
>
>
>
> Discussion of the electrical short and cracked solder joint begins on page
> 104.
>
>
>
>
>
> Best,
>
>
>
> Mike
>
>
>
> Mike Buetow
>
> PCD&F/Circuits Assembly
>
> w/m: 617-327-4702
>
> @mikebuetow
>
>
>
> The 2015 CIRCUITS ASSEMBLY *Directory of EMS Companies:*
> circuitsassembly.com/dems
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2