TECHNET Archives

December 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman     <[log in to unmask]>
Date:
Wed, 9 Dec 2015 16:03:01 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Vladimir Igoshev <[log in to unmask]>
Message-ID:
Content-Transfer-Encoding:
7bit
Subject:
From:
Vladimir Igoshev <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (104 lines)
Hi Dave,

Not really. It doesn't "burn" or "curl" much under the beam, so it's solid.

Vladimir

---- On Wed, 09 Dec 2015 15:51:29 -0800 David Hillman<[log in to unmask]> wrote ---- 
 > Thank you Steve! 
 >  
 > Vlad - does the substance slightly charge in the SEM? 
 >  
 > Dave 
 >  
 > On Wed, Dec 9, 2015 at 5:46 PM, Steve Gregory <[log in to unmask]> wrote: 
 >  
 > > Hi Dave and Vlad, 
 > > 
 > > I have it up here: 
 > > 
 > > http://stevezeva.homestead.com/What_else_it_can_be.pdf 
 > > 
 > > Steve 
 > > 
 > > On Wed, Dec 9, 2015 at 4:34 PM, David Hillman < 
 > > [log in to unmask]> wrote: 
 > > 
 > >> HI Vlad - we can't open Dropbox here due to firewall restrictions so can 
 > >> you have Steve G. post the pictures? 
 > >> 
 > >> Dave Hillman 
 > >> Rockwell Collins 
 > >> [log in to unmask] 
 > >> 
 > >> On Wed, Dec 9, 2015 at 4:59 PM, Vladimir Igoshev < 
 > >> [log in to unmask] 
 > >> > wrote: 
 > >> 
 > >> > HI everyone, 
 > >> > 
 > >> > I'm attaching a link to a file showing something I'd appreciate your 
 > >> > thoughts on. It's a cross-section of a QFN on an IAg board; 
 > >> > Pb-free/no-clean process. As you can see from the EDS spectrum, that 
 > >> > greyish stuff between pins has pretty much only Sn and O in its 
 > >> elemental 
 > >> > composition. 
 > >> > 
 > >> > I know there is burn flux residue around solder joints but that stuff 
 > >> > doesn't have any C in it. The question I have is what is it. 
 > >> > 
 > >> > I spoke to Bev and both of us are still puzzled. 
 > >> > 
 > >> > Here is the link: 
 > >> > 
 > >> https://www.dropbox.com/s/3wbj62vqjyhvj2y/What%20else%20it%20can%20be.pdf?dl=0 
 > >> > 
 > >> > Thank you very much in advance. 
 > >> > 
 > >> > Regards, 
 > >> > 
 > >> > Vladimir 
 > >> > 
 > >> > SENTEC 
 > >> > 
 > >> > 
 > >> > ______________________________________________________________________ 
 > >> > This email has been scanned by the Symantec Email Security.cloud 
 > >> service. 
 > >> > For more information please contact helpdesk at x2960 or 
 > >> [log in to unmask] 
 > >> > ______________________________________________________________________ 
 > >> > 
 > >> 
 > >> 
 > >> ______________________________________________________________________ 
 > >> This email has been scanned by the Symantec Email Security.cloud service. 
 > >> For more information please contact helpdesk at x2960 or [log in to unmask] 
 > >> ______________________________________________________________________ 
 > >> 
 > > 
 > > 
 > > 
 > > This email and any attachments are only for use by the intended 
 > > recipient(s) and may contain legally privileged, confidential, proprietary 
 > > or otherwise private information. Any unauthorized use, reproduction, 
 > > dissemination, distribution or other disclosure of the contents of this 
 > > e-mail or its attachments is strictly prohibited. If you have received this 
 > > email in error, please notify the sender immediately and delete the 
 > > original. 
 > > 
 >  
 >  
 > ______________________________________________________________________ 
 > This email has been scanned by the Symantec Email Security.cloud service. 
 > For more information please contact helpdesk at x2960 or [log in to unmask]  
 > ______________________________________________________________________ 
 > 



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2