Ravinder,
Yes, it's normal for the BGA pads on the PCB to be smaller than the BGA ball diameter - they should be about the size of the BGA package pad so that the formed joint is fairly symmetrical.
The height / diameter after reflow..... it depends. There will be some variation based on how much solder is applied and how heavy the parts is. Maybe someone has some info, but I haven't studied that closely.
Ben
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ravinder Ajmani
Sent: Thursday, December 17, 2015 4:09 PM
To: [log in to unmask]
Subject: EXTERNAL: [TN] BGA attachment to the PCB
Hi Experts,
My question is about the attachment of a BGA package to the PCB.
If the ball diameter is 0.3 mm and ball height is 0.23 mm, then what will be the final diameter and height of the balls after reflow operation. My understanding is that the balls collapse during soldering operation.
The diameter of the PCB pads is 0.25 mm. Is it normal to keep the PCB pads smaller than the BGA balls.
Thanks a lot for your help.
Regards
Ravinder Ajmani
HGST, a Western Digital company
[log in to unmask]<mailto:[log in to unmask]>
[HGST Logo]
5601 Great Oaks Parkway
San Jose, CA 95119
www.hgst.com
HGST E-mail Confidentiality Notice & Disclaimer:
This e-mail and any files transmitted with it may contain confidential or legally privileged information of HGST and are intended solely for the use of the individual or entity to which they are addressed. If you are not the intended recipient, any disclosure, copying, distribution or any action taken or omitted to be taken in reliance on it, is prohibited. If you have received this e-mail in error, please notify the sender immediately and delete the e-mail in its entirety from your system.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|