Dave,
I would recommend that you invest in a good dry box vs. cheap plastic containers that are most likely great ESD generators. Even though the PCBs themselves are not ESD sensitive, ESD components are probably located close by so any ESD generators in an electronics assembly area is not a good practice. All of our CMs including our manufacturing facility use dry boxes for temporary storage of PCBs and MSDs and they work great.
Best Regards,
Joe
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Elder
Sent: Tuesday, November 10, 2015 12:39 PM
To: [log in to unmask]
Subject: [TN] PCB storage in plastic boxes
Our production staff regularly open sealed bags, remove a few PCBs, and leave them poorly sealed. Short of then putting the remaining boards in storage cabinets, they are considering using cheap plastic containers. Does anyone have experience with this or can recommend cost-effective alternatives?
This e-mail and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as U.S. Government export controlled technical data. If you are an unintended recipient of this e-mail, use, disclosure or distribution of its content is prohibited. Please notify the sender by return e-mail and immediately delete this message.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|