About the only way to get these quickly is to buy sheet solder (readily available from Kester and Alpha) and stamp them out yourself in a small punch or arbor press.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vargas, Stephen M
Sent: Thursday, November 05, 2015 1:48 PM
To: [log in to unmask]
Subject: [TN] Solder Preforms
I have a need for some 0402 sized 63/37 solder preforms with no flux. I currently use Indium solder, but their lead time is almost 3 weeks. Any idea where I can get some of these quickly? Thanks.
Regards,
Steve Vargas
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|