Sorry, here comes new linkage for picture, please try again.
https://goo.gl/photos/jzTZVUMQoNvUvVF19
RongJun Deng
Electronics Engineer
Design Link
BB Electronics (Suzhou) Co., Ltd., EMS - from idea to solution
Block E, No.58 Yangdong Road, Loufeng, Suzhou Industrial Park- 215122 Suzhou - P.R.China
Office: +86 512 6956 2880 - Direct: +86 512 6956 0125 - Fax: +86 512 6715 7266
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Friday, October 09, 2015 11:37 PM
To: [log in to unmask]
Subject: Re: [TN] Solder joint peel off from ENIG board
opps, Many thanks for Wayne to point out. I did calculation mistake.
0.038 micron is 1.5 micro-inches. still thin. my apology... getting really old.
jk
>
Concur, IMHO, below 2uin, and depending on it's porosity, Au is unlikely
> to protect the Ni from passivating. A traditional spec would be on
> the order of 6 +/- 4uin with suppliers typically shipping at between 2
> and 3uin..
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
> Sent: Friday, October 09, 2015 5:53 AM
> To: [log in to unmask]
> Subject: Re: [TN] Solder joint peel off from ENIG board
>
> does not like to have that much gold... 0.038 micron is less than 1
> micro-inch of gold. you might have Ni oxide on surface to prevent
> good joint... you might also have some Cu oxide on the surface, if
> your Ni plating is crappy and porosity is high... can't see picture...
> did you buy cheap? (based on the amount of gold you are having).
>> EDS doesn't normally show the correct P content you begin with.Ã,
>>
>> I can not see any images.
>>
>> ââ,¬Å½Regards,
>>
>> Vladimir
>> SENTEC
>>
>> SentÃ, fromÃ, myÃ, BlackBerryÃ, 10Ã, smartphone.
>> Ã, Original Message Ã,
>> From: Deng RongJun
>> Sent: Friday, October 9, 2015 10:13
>> To: [log in to unmask]
>> Reply To: TechNet E-Mail Forum
>> Subject: [TN] Solder joint peel off from ENIG board
>>
>> Hi all:
>>
>>
>> I have got a solder joint strength issue on ENIG board, the cables
>> soldered on board can be easily detach from pads by a small external
>> force(1kg), the cable mounting process is hand soldering. Failure
>> rate is about 20%.
>>
>>
>>
>> We have made SEM and EDS test for solder joint and peel off surface,
>> P Wt% is high than normal. And we have also made SEM test for 10pcs
>> bare board, the Au thickness is 0.038-0.05um, Ni thickness is 2.8-4.0um.
>>
>>
>>
>> As I know high P Wt% will affect solder joint strength, what issue is
>> happened during PCB fabrication process? Anybody know anything about
>> this?
>>
>> Here comes pictures:
>> http://pan.baidu.com/s/1sjl7Ynb
>>
>> Best regards
>> Deng
>>
>> _____________________________________________________________________
>> _ This email has been scanned by the Symantec Email Security.cloud
>> service.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> _____________________________________________________________________
>> _
>>
>> _____________________________________________________________________
>> _ This email has been scanned by the Symantec Email Security.cloud
>> service.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> _____________________________________________________________________
>> _
>>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|