TECHNET Archives

October 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ed Popielarski <[log in to unmask]>
Date:
Fri, 2 Oct 2015 12:45:06 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (219 lines)
cool.
> Nah.. UHF broadcast. Over the air pay-TV in NJ, Wometco Home Theater @
> Blonder-Tongue Labs. 8db Horiz. Sync suppression and L-R mpx for program
> audio, zero X-ing for h.sync restoration by bumping RF gain resides in the
> pilot tone. https://en.wikipedia.org/wiki/Wometco_Home_Theater
>
>
> Ed Popielarski
> Engineering Manager
>
>
>                                970 NE 21st Ct.
>                               Oak Harbor, Wa. 98277
>
>                               Ph: 360-675-1322
>                               Fx: 206-624-0695
>                               Cl: 949-581-6601
>
>
>
>        "It's one kind of victory to slay a beast, move a mountain, and
> cross a chasm, but it's another kind altogether to realize that the
> beast, the mountain, and the chasm were of your own design."
> https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
>
>
> -----Original Message-----
> From: [log in to unmask] [mailto:[log in to unmask]]
> Sent: Friday, October 02, 2015 9:14 AM
> To: TechNet E-Mail Forum; Ed Popielarski
> Subject: Re: [TN] Solder mask removal, SMOBC
>
> working on mm wave bands?  19 GHz?
>                    jk
>> Nope. Clawed my way up from RF R&D tech back in the late 70's.
>>
>> Ed Popielarski
>> Engineering Manager
>>
>>
>>                                970 NE 21st Ct.
>>                               Oak Harbor, Wa. 98277
>>
>>                               Ph: 360-675-1322
>>                               Fx: 206-624-0695
>>                               Cl: 949-581-6601
>>
>>
>>
>>        "It's one kind of victory to slay a beast, move a mountain, and
>> cross a chasm, but it's another kind altogether to realize that the
>> beast, the mountain, and the chasm were of your own design."
>> https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&s
>> pn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
>>
>>
>> -----Original Message-----
>> From: [log in to unmask] [mailto:[log in to unmask]]
>> Sent: Friday, October 02, 2015 8:50 AM
>> To: TechNet E-Mail Forum; Ed Popielarski
>> Subject: Re: [TN] Solder mask removal, SMOBC
>>
>> you mean you are the "pure manager" without the engineering part?
>> LOL.
>>                jk
>>> Hey now... I quit several months ago (and damned proud of it after
>>> 40+ years)... cut me a little slack, bud! LOL
>>>
>>> Ed Popielarski
>>> Engineering Manager
>>>
>>>
>>>                                970 NE 21st Ct.
>>>                               Oak Harbor, Wa. 98277
>>>
>>>                               Ph: 360-675-1322
>>>                               Fx: 206-624-0695
>>>                               Cl: 949-581-6601
>>>
>>>
>>>
>>>        "It's one kind of victory to slay a beast, move a mountain,
>>> and cross a chasm, but it's another kind altogether to realize that
>>> the beast, the mountain, and the chasm were of your own design."
>>> https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&
>>> s pn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
>>>
>>>
>>> -----Original Message-----
>>> From: Stadem, Richard D. [mailto:[log in to unmask]]
>>> Sent: Friday, October 02, 2015 8:19 AM
>>> To: Ed Popielarski; TechNet E-Mail Forum
>>> Subject: RE: Solder mask removal, SMOBC
>>>
>>> Yes, and they would have the proper environmental controls and safety
>>> equipment, etc.
>>> Even if you attempted to remove it using a conformal coat blaster,
>>> you still have the safety issues to deal with. You don't want to
>>> breathe that stuff.
>>> Excuse me while I go outside for a cigarette.
>>> Odin
>>>
>>> -----Original Message-----
>>> From: Ed Popielarski [mailto:[log in to unmask]]
>>> Sent: Friday, October 02, 2015 10:16 AM
>>> To: TechNet E-Mail Forum; Stadem, Richard D.
>>> Subject: RE: Solder mask removal, SMOBC
>>>
>>> In addition to Richard's sage advice and rationalization is the fact
>>> they are set up to deal with harsh chemistry like this and probably
>>> do so on a regular basis.
>>>
>>> Ed Popielarski
>>> Engineering Manager
>>>
>>>
>>>                                970 NE 21st Ct.
>>>                               Oak Harbor, Wa. 98277
>>>
>>>                               Ph: 360-675-1322
>>>                               Fx: 206-624-0695
>>>                               Cl: 949-581-6601
>>>
>>>
>>>
>>>        "It's one kind of victory to slay a beast, move a mountain,
>>> and cross a chasm, but it's another kind altogether to realize that
>>> the beast, the mountain, and the chasm were of your own design."
>>> https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&
>>> s pn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
>>>
>>>
>>> -----Original Message-----
>>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
>>> Sent: Friday, October 02, 2015 5:36 AM
>>> To: [log in to unmask]
>>> Subject: Re: [TN] Solder mask removal, SMOBC
>>>
>>> Perhaps you can ask your board fabricator? I would imagine they have
>>> methods for doing this. Perhaps also they may be able to do it for
>>> you cheaper than you could set yourself up to do it? Doesn't hurt to
>>> ask.
>>>
>>> -----Original Message-----
>>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
>>> Sent: Friday, October 02, 2015 6:52 AM
>>> To: [log in to unmask]
>>> Subject: [TN] FW: Solder mask removal, SMOBC
>>>
>>> Fellow TechNetters:
>>>
>>>    I did not receive very much feedback on my initial inquiry.
>>> Therefore, I ask again.   Additionally I also ask if Solder mask and
>>> conformal coating the same Product/Term (IPC-7711.21  section 2.3.1.
>>> I want to removal/strip solder mask.   At this point I do not known the
>>> solder mask vendor or type.
>>>
>>> Victor,
>>>
>>> From: Hernandez, Victor G
>>> Sent: Thursday, October 01, 2015 10:56 AM
>>> To: TechNet E-Mail Forum
>>> Cc: Hernandez, Victor G
>>> Subject: Solder mask removal
>>>
>>> Fellow TechNetters:
>>>
>>>    I have been asked to see if that is a satisfactory method for
>>> removing/stripping solder mask from sample coupons chemically and/or
>>> mechanically.
>>>
>>> Victor,
>>>
>>>
>>> _____________________________________________________________________
>>> _ This email has been scanned by the Symantec Email Security.cloud
>>> service.
>>> For more information please contact helpdesk at x2960 or
>>> [log in to unmask]
>>> _____________________________________________________________________
>>> _
>>>
>>> _____________________________________________________________________
>>> _ This email has been scanned by the Symantec Email Security.cloud
>>> service.
>>> For more information please contact helpdesk at x2960 or
>>> [log in to unmask]
>>> _____________________________________________________________________
>>> _
>>>
>>> _____________________________________________________________________
>>> _ This email has been scanned by the Symantec Email Security.cloud
>>> service.
>>> For more information please contact helpdesk at x2960 or
>>> [log in to unmask]
>>> _____________________________________________________________________
>>> _
>>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud
>> service.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2