My first thoughts were the age of the material. First question was how old is the board? Second question was how old was the material used to fabricate the board? The other questions that were asked below are good one's too.
Mick
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Francis Byle
Sent: Wednesday, October 28, 2015 12:15 PM
To: [log in to unmask]
Subject: Re: [IPC-600-6012] Flex quesstion
I have never seen anything quite like this... the image does raise some questions, however:
* What is the age of the flex section depicted. Is this new product, or a field failure?
* What kind of thermal and vibe history has the flex seen?
* What is the thickness of the flex section, and how many layers are present?
* Is the source of the fine surface scratches running roughly horizontally in the imge known?
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Hammill, Vicka (EHCOE)
Sent: Wednesday, October 28, 2015 10:56
To: [log in to unmask]
Subject: [IPC-600-6012] Flex quesstion
Has anyone ever seen this condition of cracking of the Kapton on a flexible part of a rigid flex? If so, do you the cause? We have done crossections on this and it showed the kapton only cracking...the adhesive was not cracked and remained untouched. So far, we have found no specific reason for the cause.
Any input would be appreciated.
Vicka Hammill
Staff Engineer/PB CAA
Honeywell
Lync Phone: 480-627-5547
FAX: 602-436-1005
[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]:[log in to unmask]>>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
|
|
|