TECHNET Archives

October 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Mike Fenner <[log in to unmask]>
Date:
Fri, 16 Oct 2015 16:34:35 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Message-ID:
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
<42F4B88CC51543449A617BA59636D67B@MikePC>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (114 lines)
Good idea! That is one I will try to remember if I ever run into that problem. Thanks for a good tip, Mike.
dean

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: Friday, October 16, 2015 9:40 AM
To: [log in to unmask]
Subject: Re: [TN] soldering to stainless

If you are soldering the SS to an electronic assembly it might be worth considering pre-tinning using the aggressive flux first while it is still a piece of structural stuff. Now you can handle it more easily, do your aggressive cleaning and drying without fear of damaging your electronics.
The pre-tinned SS can then be reflowed using ordinary no clean, rosin or whatever flux type you are using.

--
Regards 
 
Mike 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Nutting, Phil
Sent: Friday, October 16, 2015 2:07 PM
To: [log in to unmask]
Subject: Re: [TN] soldering to stainless

We had to solder drain wires to stainless steel transformer shields.  We used LA-CO N-3 flux purchased from McMaster-Carr.  I have since used it for many other stainless soldering applications with great success.  Even soldered stainless wire mesh to sheet stainless... awesome.  The caveat is to remove ALL the flux as it is quite aggressive.  We learned that when a CM didn't properly clean the flux residue and we ended up with lateen failures Once cleaned you can't tell the difference in the solder joint.

Phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman
Sent: Friday, October 16, 2015 8:28 AM
To: [log in to unmask]
Subject: Re: [TN] soldering to stainless

Hi Guy! You will want to look at the OR and IN flux classifications for soldering stainless steel as you will need a highly aggressive flux material to accomplish the task. I have received good counseling from the folks at Indium and Superior Flux on a couple of applications where I needed that kind of flux power. Many of the IN fluxes " can solder concrete" so keep a focus on your cleaning process after soldering. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]

On Fri, Oct 16, 2015 at 7:14 AM, Guy Ramsey <[log in to unmask]> wrote:

> Will any of the fluxes classified to J-004 yield good solder 
> connection to stainless steel?
>
>
>
>
>
> cid:[log in to unmask]
>
> Guy Ramsey | R&D Interconnect Solutions | Process Manager |
>
>  <mailto:[log in to unmask]> [log in to unmask] | Mobile:  610-349-2519 |
> Office:
> 610-443-2299 |
> 1660 East Race Street  | Allentown, PA 18109 USA | 
> <http://www.rdis.com/> www.rdis.com
>
>
>
>
>
> The contents of this email and any attachments to it contain 
> confidential and/or legally privileged information from R&D Altanova.
> This information is only for the use of the intended recipient. If you 
> are not the intended recipient, you are hereby notified that any 
> disclosure, copying, distribution, or the taking of any action in 
> reliance on the comments of the contained information is strictly 
> prohibited and that the email and any attachments thereto should be 
> returned to R&D Altanova immediately. In this regard, if you have 
> received this document in error, please notify us by email 
> immediately.
>
>
>
> **Although this email and any attachments are believed to be free of 
> any virus or other defect that might affect any computer system into 
> which it is received and opened, it is the responsibility of the 
> recipient to ensure that the email is virus free. R&D Altanova accepts 
> no responsibility for any loss or damage arising in any way from use 
> of the email.
>
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2