I used to use simple hi-temperature lithium grease for that application and it worked very well.
Just be sure your machine is no longer under warranty, as using anything other than what they recommend during the warranty period could void it.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, October 13, 2015 11:07 AM
To: [log in to unmask]
Subject: [TN] Lubrication for wave solder pot lift spindles
Hi All!
Our maintenance technician just came to me with a quote he got from Vitronics/Soltec for some lube for the wave solder pot spindles (the ones that raise and lift the solder pot), and I about crapped my pants! They want $729.64 for a 400-gram tube!! Holy cow! Do any of you know of any other grease that is more reasonable that works good? I just can't see paying that much for grease...
Steve
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|