are you sure it is not glass passivation scratch? The cct might be a bit
on the high side, it could skipped damage, but the other may have chip
out?
> Hi Julie,
>
> Have your photo up, it's here:
>
> http://stevezeva.homestead.com/3CK_2nd_decap_-_multiview.jpg
>
> Steve
>
> On Thu, Oct 8, 2015 at 10:21 AM, Julie Silk <[log in to unmask]>
> wrote:
>
>> We had an intermittent failure on a part and after decap, there was a
>> rope-like line that seemed to weave in and out of the circuitry. I'm
>> having Steve Gregory post a picture. I'd like your thoughts on what is
>> going on. We're consulting with the supplier, but I'd like your input.
>>
>
> --
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential, proprietary
> or otherwise private information. Any unauthorized use, reproduction,
> dissemination, distribution or other disclosure of the contents of this
> e-mail or its attachments is strictly prohibited. If you have received
> this
> email in error, please notify the sender immediately and delete the
> original.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|