TECHNET Archives

October 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 29 Oct 2015 20:27:38 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Vladimir Igoshev <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
MIME-Version:
1.0
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (55 lines)
I was waiting for you to spell it out :-)

Vladimir
SENTEC

Sent from my BlackBerry 10 smartphone on the Rogers network.
  Original Message  
From: Bev Christian
Sent: Thursday, October 29, 2015 20:10
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: Re: [TN] No-wetting on Mini USB (Nickel plating)

Deng,
I suggest if you have the time, get the supplier to provide you connectors with a tin or solder plating already on the connection pins. 

About a decade ago almost lost my job over these suckers. Told my boss that the USB connectors were bare nickel and he brushed it off and we had terrible field problems as a result.
Bev
Blackberry

Opinions expressed are my own and may not represent those of the company I work for.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Deng RongJun
Sent: October 29, 2015 3:33 AM
To: [log in to unmask]
Subject: [TN] No-wetting on Mini USB (Nickel plating)

Hi Technetters

I have got a problem with a SMT type mini USB connector. The four pins contacted shield are no-wetting after reflow soldering. But can be solder well by iron.
The pins only plated by Nickel, is it possible the oxidation film creating on pin surface and then affect soldering? 

Picture:
https://goo.gl/photos/qap1CBEWzUEJEc5i6

Thanks in advance.

RongJun Deng


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2