If Chlorox really does contain ionic chlorides and they are not removed then
they could contribute to static dissipation on testing. That would make your
tests somewhat false.
--
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Louis Hart
Sent: Wednesday, October 21, 2015 1:13 PM
To: [log in to unmask]
Subject: Re: [TN] ESD concern
The people who make the mats must have some recommended or approved cleaner.
Following up on Ioan's comment, chlorine can diffuse through the seal of an
aluminum electrolytic capacitor and corrode the electrodes and connections.
The chlorine is not consumed in the reaction, so the smallest amount will
eventually destroy the part. Louis Hart
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Sue Powers-Hartman
Sent: Tuesday, October 20, 2015 6:57 PM
To: [log in to unmask]
Subject: [TN] ESD concern
We usually clean the ESD work tables with a product called Reztore. Now
some employees feel that this product is not getting the tables clean enough
so they are using Clorox wipes. Will this strip the ESD properties from the
table top? If they use the Clorox wipes and then come after and wipe down
with Reztore, would that be acceptable.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|