Yes, it certainly is, especially to me as geology is one of my favorite hobbies.
Thanks, Ed!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Wednesday, September 16, 2015 2:21 PM
To: [log in to unmask]
Subject: Re: [TN] ENEPIG Question?
Cool photo!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski
Sent: Wednesday, September 16, 2015 2:53 PM
To: [log in to unmask]
Subject: Re: [TN] ENEPIG Question?
http://www.mindat.org/photo-33512.html
Ed Popielarski
Engineering Manager
970 NE 21st Ct.
Oak Harbor, Wa. 98277
Ph: 360-675-1322
Fx: 206-624-0695
Cl: 949-581-6601
"It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design."
https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, September 16, 2015 10:59 AM
To: [log in to unmask]
Subject: Re: [TN] ENEPIG Question?
That is correct, but only to a point. If something is, in fact, physically measureable, then it pertains to a real fact or a real relational finding. If the measurement is based on a hypothesis as yet disproven, then the derived measurement is not a real fact. If you tell me you know, for a fact, something based on a hypothetical method of measurement (an implied result), then I can just as safely assume that you are full of radioactive isotopes from the planet Beryl.
Well, you folks wanted to keep this string going, so I have done my part.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
Sent: Wednesday, September 16, 2015 12:31 PM
To: [log in to unmask]
Subject: Re: [TN] ENEPIG Question?
It would be similar to one formed on ENIG. ANYTHING CAN BE MEASURED.
Vladimir
Sent from my BlackBerry 10 smartphone on the Rogers network.
Original Message
From: Victor Hernandez
Sent: Wednesday, September 16, 2015 13:10
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: Re: [TN] ENEPIG Question?
Can this IMC formation be measured at a microscopic level?
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: Wednesday, September 16, 2015 12:01 PM
To: [log in to unmask]
Subject: Re: [TN] ENEPIG Question?
Jeffrey,
Pd also dissolves into the joint, and again you are forming an intermetallic with the nickel.
Ben
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jenkins, Jeffrey A @ CSG - LINKABIT
Sent: Wednesday, September 16, 2015 12:02 PM
To: [log in to unmask]
Subject: EXTERNAL: [TN] ENEPIG Question?
Hi All,
Quick question, with an ENIG finish, I know the gold dissolves into the joint and we solder to the Ni.
But what about ENEPIG? I'm assuming the Au will dissolve, but what happen with the Pd? Does it stay put or also dissolve into the joint?
Inquiring minds want to know.
Thanks,
-Jeffrey
Jeffrey A. Jenkins
Sr. PCB Staff Designer, CID+/CIT
L-3 Communications, Linkabit Division
Work: 858-552-9832
Email: [log in to unmask]
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
________________________________
“Confidentiality Notice:
This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments.”
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|