Hi Adrian,
Although I concur with our colleagues that, for your volumes, masking/spraying should be reliable and cost effective, it seems that your original question has not been answered. So here's, in my personal order of preference, a list of selective coating equipment manufacturers:
http://www.pva.net/
http://www.nordson.com/en-us/divisions/asymtek/pages/default.aspx
http://www.nordsonefd.com/ca/
PVA and Asymtek provide full size and capability machines, whereas EFD might help with one of their tabletop robots.
They all provide precious info on equipment and valve selection, related to your application. They can also develop the process you need and provide you with an optimized program.
Best regards,
Ioan Tempea, P. Eng.
Manufacturing Engineer, Satellite Systems
MacDonald, Dettwiler and Associates Corporation, 21025 Trans-Canada Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2
Tel: +1-514-457-2150 x3556
www.mdacorporation.com<http://www.mdacorporation.com>
This e-mail, and any attachments, are intended solely for the use of the intended recipient(s) and may contain legally privileged, proprietary and/or confidential information. Any use, disclosure, dissemination, distribution or copying of this e-mail and any attachments for any purposes that have not been specifically authorized by the sender is strictly prohibited. If you are not the intended recipient, please immediately notify the sender by reply e-mail and permanently delete all copies and attachments. This email is for informational purposes only and shall not be interpreted to authorize or conclude a binding agreement between MDA and any other party unless this email contains or is accompanied by an express written confirmation of MDA's intention to enter into a binding agreement, such confirmation shall only be provided by an authorized representative of MDA.
-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de Adrian Dimulescu Envoyé : Thursday, September 03, 2015 10:39 AM À : [log in to unmask] Objet : [TN] Selective Conformal Coat Systems
Hello All,
We're looking into purchasing a small (bench-top type) automated selective conformal coat system. This will be used for 100 or so boards a week, therefore speed is not an issue. It is important that the system is selective as we only want to coat specific areas on the board. I wanted to get a feel for what other are using and/or recommend.
Many Thanks
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
________________________________
Adrian Dimulescu | Advanced Engineer | MtronPTI (NYSE MKT: LGL)
2525 Shader Rd, Orlando, FL 32804
Office: 407.298.2000
CONFIDENTIALITY NOTICE:
This email together with any attachments is confidential; intended for only the
recipient(s) named above and may contain information that is privileged or
exempt from disclosure under applicable law. If you have received this email in
error, or are not the named recipient(s), you are hereby notified that any use,
dissemination, distribution or copying of this email or any attachments is
strictly prohibited. Please immediately notify the sender and delete this email
and any attachments from your computer. You should not retain, copy or use this
email or any attachments for any purpose, or disclose all or any part of the
contents to any person. The LGL Group, Inc. and its subsidiaries reserve the
right to monitor all email communications through its networks.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|