A larger solder joint can present itself to a shear load, as in the case of a large mismatch in CTEs, as a greater risk of catastrophic cracking than a smaller and more ductile solder joint. The height (h in the Engelmair/Wild equation) has much more of an effect than the overall size or volume. While the strength is directly proportional to the pad size in terms of being able to shear through a fixed mound of solder, it is not necessarily more reliable in terms of fracturing from the base.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Deng RongJun
Sent: Thursday, September 24, 2015 8:30 PM
To: [log in to unmask]
Subject: Re: [TN] Component solder reliability
Hi Bev:
As I know the solder joint strength directly proportional to pad size, is that not correct?
RongJun Deng
Electronics Engineer
Design Link
From: Bev Christian [mailto:[log in to unmask]]
Sent: Friday, September 25, 2015 8:49 AM
To: 'TechNet E-Mail Forum' <[log in to unmask]>; Deng RongJun <[log in to unmask]>
Subject: RE: [TN] Component solder reliability
Rongjun,
If Werner Engelmaier were still alive he would shake his finger at you! :)
Solder joint strength is not necessarily a sign of a reliable joint. It might or might not mean that a joint is well made but not say much about reliability. For instance Ericsson (I believe) found that small (lower shear strength) solder joints for chip components were actually better because they were more ductile.
That is why you will never find an official published list of pass/fail solder joint strengths.
Bev
Blackberry
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Deng RongJun
Sent: September 24, 2015 3:31 AM
To: [log in to unmask]
Subject: [TN] Component solder reliability
Hi Experts:
Is there have an industry standard for component pull/push test? What is standard value for each component?
RongJun Deng
Electronics Engineer
Design Link
BB Electronics (Suzhou) Co., Ltd., EMS - from idea to solution
Block E, No.58 Yangdong Road, Loufeng, Suzhou Industrial Park- 215122 Suzhou - P.R.China
Office: +86 512 6956 2880 - Direct: +86 512 6956 0125 - Fax: +86 512 6715 7266
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|