Subject: | |
From: | |
Reply To: | |
Date: | Thu, 24 Sep 2015 13:34:44 +0200 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Hello RongJun
You may find info about test methods on following IEC standard:
- Shear test : IEC 62137-1-2
- Pull test : IEC 62137-1-1
Above standards don't report values, that depends from a lot of
variables such land surface, pin dimension, and more
Regards
Francesco
Il 24/09/2015 9.30, Deng RongJun ha scritto:
> Hi Experts:
>
>
>
> Is there have an industry standard for component pull/push test? What is standard value for each component?
>
>
>
>
>
> RongJun Deng
>
> Electronics Engineer
>
> Design Link
>
> BB Electronics (Suzhou) Co., Ltd., EMS - from idea to solution
>
>
>
> Block E, No.58 Yangdong Road, Loufeng, Suzhou Industrial Park- 215122 Suzhou - P.R.China
>
> Office: +86 512 6956 2880 - Direct: +86 512 6956 0125 - Fax: +86 512 6715 7266
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
--
Francesco Di Maio
IPC e Formazione
IPC A-600, IPC A-610, IPC 7711/21 Certified IPC Trainer
Via Kennedy Ingresso 2, 20871 Vimercate (MB) - Italy
Desk:+39.03989085921 - Mobile: +39.3206877284 - Fax: +39.03989085051
E-Mail:[log in to unmask]
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|