Its basically a thermoplastic material used for mounting bare die, Crystalbond
is a trade name.
Make sure the Tg temperature of the thermoplastic doesn't degrade the part being
mounted.
On 9/14/2015 10:29 AM, Victor Hernandez wrote:
> Fellow TechNetters:
>
> In a previous life, the other Big Blue, I used a product referred to as "Bees Wax" for mounting ICs onto a sample holder for polishing. A small amount of bees wax was melted and then the IC placed over it and let to dry. The IC would not move on the holder till reheated. Does anyone out there have a real name and part number for this product and where I can purchase it... I currently have a need to use it in a different application.
>
> Victor,
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
--
Bhanu Sood
Center for Advanced Life Cycle Engineering (CALCE)
Test Services and Failure Analysis Laboratory
University of Maryland
Room 0128, 4298 Campus Dr. (Bldg. 88)
College Park, MD 20742 USA
Tel: +1 (301) 405 3498
Fax: +1 (301) 314 9269
e-mail: [log in to unmask]
Skype: calce_umd
website: www.calce.umd.edu/TSFA
Confidentiality Notice: The information contained in this e-mail and
any attachments may be legally privileged and confidential. If you are not
an intended recipient, you are hereby notified that any dissemination,
distribution or copying of this e-mail is strictly prohibited.
If you have received this e-mail in error, please notify the sender
and permanently delete the e-mail and any attachments immediately.
You should not retain, copy or use this e-mail or any attachment
for any purpose, nor disclose all or any part of the contents to any
other person.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|