Yes, there are several different temporary mounting adhesives available. The
water soluble one is useful for low temp apps.
Crystalbond - low to medium temperature, acetone strips residue
revAlpha - Dry process, versions made up to 150C, heat release, no residue
There's also a UV releasable material for temporary mounts on UV-transparent
glass. I haven't used it, but I believe it can go through reflow.
Wayne
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of lduso - Diamond-MT.com
Sent: Monday, September 14, 2015 10:36 AM
To: [log in to unmask]
Subject: Re: [TN] Bees wax
Sounds like something similar to Carbowax
<http://t.sidekickopen03.com/e1t/c/5/f18dQhb0S7lC8dDMPbW2n0x6l2B9nMJN7t5XYgdVhPKW4WYq3x5wvpw0W7fRL1x56dPnsf3Pj9QP02?t=http%3A%2F%2Fwww.dow.com%2Fpolyglycols%2Fpolyethylene%2Fproducts%2Fcarbowaxp.htm&si=6019012419387392&pi=fd0f4423-7ac1-40b8-8baa-28c085394e40>.
Water soluble wax that we have used for masking parylene.
Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com
On Mon, Sep 14, 2015 at 10:29 AM, Victor Hernandez <
[log in to unmask]> wrote:
> Fellow TechNetters:
>
> In a previous life, the other Big Blue, I used a product referred to as
> "Bees Wax" for mounting ICs onto a sample holder for polishing. A small
> amount of bees wax was melted and then the IC placed over it and let to
> dry. The IC would not move on the holder till reheated. Does anyone out
> there have a real name and part number for this product and where I can
> purchase it... I currently have a need to use it in a different
> application.
>
> Victor,
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|