That sounds more like the problem, masking technique. We mask hundreds a
day and rarely damage anything. It's all in using the right technique and
as Steve said, the right material.
What coating are you using?
Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com
On Thu, Sep 3, 2015 at 10:43 AM, Adrian Dimulescu <[log in to unmask]>
wrote:
> That’s what we’re doing now, the issue is removing the mask as it will
> occasionally lift a pad or component. We’re looking to do away with
> masking.
>
>
>
> Thanks
>
>
>
> ------------------------------
> *Adrian Dimulescu | Advanced Engineer | MtronPTI (NYSE MKT: LGL)*
> 2525 Shader Rd, Orlando, FL 32804
> Office: 407.298.2000
>
>
>
> *From:* lduso - Diamond-MT.com [mailto:[log in to unmask]]
> *Sent:* Thursday, September 03, 2015 10:41 AM
> *To:* TechNet E-Mail Forum; Adrian Dimulescu
> *Subject:* Re: [TN] Selective Conformal Coat Systems
>
>
>
> That low a volume, mask and spray by hand.
>
>
> Lloyd Duso
>
> Diamond-MT
> Plant Manager
> (814) 535-3505
>
> www.Diamond-mt.com
>
>
>
> On Thu, Sep 3, 2015 at 10:39 AM, Adrian Dimulescu <[log in to unmask]>
> wrote:
>
> Hello All,
>
> We're looking into purchasing a small (bench-top type) automated selective
> conformal coat system. This will be used for 100 or so boards a week,
> therefore speed is not an issue. It is important that the system is
> selective as we only want to coat specific areas on the board. I wanted to
> get a feel for what other are using and/or recommend.
>
> Many Thanks
>
>
>
> CONFIDENTIALITY NOTICE:
> This email together with any attachments is confidential; intended for only the
> recipient(s) named above and may contain information that is privileged or
> exempt from disclosure under applicable law. If you have received this email in
> error, or are not the named recipient(s), you are hereby notified that any use,
> dissemination, distribution or copying of this email or any attachments is
> strictly prohibited. Please immediately notify the sender and delete this email
> and any attachments from your computer. You should not retain, copy or use this
> email or any attachments for any purpose, or disclose all or any part of the
> contents to any person. The LGL Group, Inc. and its subsidiaries reserve the
> right to monitor all email communications through its networks.
>
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|