No arguing there :-)
Sent from my BlackBerry 10 smartphone on the Rogers network.
Original Message
From: Stewart McCracken
Sent: Wednesday, September 16, 2015 13:54
To: 'TechNet E-Mail Forum'; [log in to unmask]
Subject: RE: [TN] ENEPIG Question?
My point really - depends on what you can see... ; )
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
Sent: 16 September 2015 18:51
To: [log in to unmask]
Subject: Re: [TN] ENEPIG Question?
If you don't see it than it's probably not there and there is nothing to measure :-)
Vladimir
Sent from my BlackBerry 10 smartphone on the Rogers network.
Original Message
From: Stewart McCracken
Sent: Wednesday, September 16, 2015 13:46
To: 'TechNet E-Mail Forum'; [log in to unmask]
Subject: RE: [TN] ENEPIG Question?
assuming you can see it / detect it... ; )
Stewart
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
Sent: 16 September 2015 18:31
To: [log in to unmask]
Subject: Re: [TN] ENEPIG Question?
It would be similar to one formed on ENIG. ANYTHING CAN BE MEASURED.
Vladimir
Sent from my BlackBerry 10 smartphone on the Rogers network.
Original Message
From: Victor Hernandez
Sent: Wednesday, September 16, 2015 13:10
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: Re: [TN] ENEPIG Question?
Can this IMC formation be measured at a microscopic level?
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: Wednesday, September 16, 2015 12:01 PM
To: [log in to unmask]
Subject: Re: [TN] ENEPIG Question?
Jeffrey,
Pd also dissolves into the joint, and again you are forming an intermetallic with the nickel.
Ben
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jenkins, Jeffrey A @ CSG - LINKABIT
Sent: Wednesday, September 16, 2015 12:02 PM
To: [log in to unmask]
Subject: EXTERNAL: [TN] ENEPIG Question?
Hi All,
Quick question, with an ENIG finish, I know the gold dissolves into the joint and we solder to the Ni.
But what about ENEPIG? I'm assuming the Au will dissolve, but what happen with the Pd? Does it stay put or also dissolve into the joint?
Inquiring minds want to know.
Thanks,
-Jeffrey
Jeffrey A. Jenkins
Sr. PCB Staff Designer, CID+/CIT
L-3 Communications, Linkabit Division
Work: 858-552-9832
Email: [log in to unmask]
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|