Dear Technetters:
Had the following question from a client today...
*...... a question regarding damaged conductors (nicks and scrapes >10%). *
*I have a 7 stranded wire that is cut and stripped by an outside supplier
that has multiple wires coming in either nicked or scraped >10% resulting
in a defect condition. My question is what is the reasoning or
justification behind this accept/reject criteria?*
* I can guess that it may have some limitations regarding current carrying
capabilities or are subject to latent defects ( severed ) conditions due to
the end use environment/vibration, corrosive etc.. *
*My answer has to do this is:*
The ampacity for the conductor is a function of the material (copper or
aluminum for example) and is based on its physical and electrical
properties of the material. It is the current which can be carried such
that the material would not up and be destroyed. The absolute value of this
is a function of the amount of material (a nicked conductor would have less
ampacity) and the reasons that the maximum deterioration was chosen to be
10% was <????>
Maybe this iso ne of those times, just like you tell your children, just
because!
Bob Wettermann
BEST Inc
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|