TECHNET Archives

September 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 16 Sep 2015 18:29:35 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Stewart McCracken <[log in to unmask]>
Subject:
From:
Stewart McCracken <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (76 lines)
Yes, IMC layers readily measurable from a few tens of nm. Careful x-section prep needed, can identify most elements of interest at sub-micron level using EDS also.  

Stewart


Stewart McCracken

Managing Director | MCS | Solving your Materials, Manufacturing and Reliability Issues
[log in to unmask] | www.themcsgroup.co.uk | +44(0)131 440 9090 | +44(0)771 154 1735

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: 16 September 2015 18:05
To: [log in to unmask]
Subject: Re: [TN] ENEPIG Question?

Can this IMC formation be measured at a microscopic level?

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: Wednesday, September 16, 2015 12:01 PM
To: [log in to unmask]
Subject: Re: [TN] ENEPIG Question?

Jeffrey,

Pd also dissolves into the joint, and again you are forming an intermetallic with the nickel.

Ben

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jenkins, Jeffrey A @ CSG - LINKABIT
Sent: Wednesday, September 16, 2015 12:02 PM
To: [log in to unmask]
Subject: EXTERNAL: [TN] ENEPIG Question?

Hi All,

Quick question, with an ENIG finish, I know the gold dissolves into the joint and we solder to the Ni.

But what about ENEPIG? I'm assuming the Au will dissolve, but what happen with the Pd? Does it stay put or also dissolve into the joint?

Inquiring minds want to know.

Thanks,

-Jeffrey

Jeffrey A. Jenkins
Sr. PCB Staff Designer, CID+/CIT
L-3 Communications, Linkabit Division
Work:  858-552-9832
Email:  [log in to unmask]



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2