We tried water soluble mask, but it created a lot of problems with our D.I. wash.
Experience the benefits of Precision Engagement
Brien Bush
Manufacturing Applications Specialist
Phone: 603.249.9190 | Fax: 603.249.9192
[log in to unmask] www.cirtronics.com
ISO 9001 & 13485 Certified
Follow us on LinkedIn|Friend us on Facebook
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Tuesday, September 15, 2015 12:39 PM
To: [log in to unmask]
Subject: [TN] Water soluble masking materials - Bayesian Filter detected spam
A quick question for you all. Are any of you using a water soluble masking material, like a Kester Wondermask, in your wave solder or selective solder operations? If so, what are you using?
Doug Pauls
Principal Materials and Process Engineer Rockwell Collins
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
WARNING: Export Control This message, including any attachments, may contain technical data within the definition of the International Traffic in Arms Regulations (ITAR), and subject to the Export Control Laws of the U.S. Government. Transfer of such information by any means to a foreign person, whether in the United States or abroad, without proper export authorization or other approval from the U.S. Department of State is prohibited.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|