TECHNET Archives

September 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "lduso - Diamond-MT.com" <[log in to unmask]>
Date:
Thu, 3 Sep 2015 10:00:32 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Douglas Pauls <[log in to unmask]>
Message-ID:
Subject:
From:
Douglas Pauls <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (118 lines)
I agree with Lloyd, if you are damaging components during demask, you are
using the wrong materials and the wrong techniques.

Trot them out here where we can see em and we'll help ya out.


Doug Pauls
Principal Materials and Process Engineer
Rockwell Collins

On Thu, Sep 3, 2015 at 9:55 AM, lduso - Diamond-MT.com <[log in to unmask]
> wrote:

> That sounds more like the problem, masking technique. We mask hundreds a
> day and rarely damage anything. It's all in using the right technique and
> as Steve said, the right material.
>
> What coating are you using?
>
> Lloyd Duso
> Diamond-MT
> Plant Manager
> (814) 535-3505
> www.Diamond-mt.com
>
> On Thu, Sep 3, 2015 at 10:43 AM, Adrian Dimulescu <[log in to unmask]
> >
> wrote:
>
> > That’s what we’re doing now, the issue is removing the mask as it will
> > occasionally lift a pad or component.  We’re looking to do away with
> > masking.
> >
> >
> >
> > Thanks
> >
> >
> >
> > ------------------------------
> > *Adrian Dimulescu | Advanced Engineer | MtronPTI (NYSE MKT: LGL)*
> > 2525 Shader Rd, Orlando, FL 32804
> > Office: 407.298.2000
> >
> >
> >
> > *From:* lduso - Diamond-MT.com [mailto:[log in to unmask]]
> > *Sent:* Thursday, September 03, 2015 10:41 AM
> > *To:* TechNet E-Mail Forum; Adrian Dimulescu
> > *Subject:* Re: [TN] Selective Conformal Coat Systems
> >
> >
> >
> > That low a volume, mask and spray by hand.
> >
> >
> > Lloyd Duso
> >
> > Diamond-MT
> > Plant Manager
> > (814) 535-3505
> >
> > www.Diamond-mt.com
> >
> >
> >
> > On Thu, Sep 3, 2015 at 10:39 AM, Adrian Dimulescu <
> [log in to unmask]>
> > wrote:
> >
> > Hello All,
> >
> > We're looking into purchasing a small (bench-top type) automated
> selective
> > conformal coat system.  This will be used for 100 or so boards a week,
> > therefore speed is not an issue.  It is important that the system is
> > selective as we only want to coat specific areas on the board.  I wanted
> to
> > get a feel for what other are using and/or recommend.
> >
> > Many Thanks
> >
> >
> >
> > CONFIDENTIALITY NOTICE:
> > This email together with any attachments is confidential; intended for
> only the
> > recipient(s) named above and may contain information that is privileged
> or
> > exempt from disclosure under applicable law. If you have received this
> email in
> > error, or are not the named recipient(s), you are hereby notified that
> any use,
> > dissemination, distribution or copying of this email or any attachments
> is
> > strictly prohibited. Please immediately notify the sender and delete
> this email
> > and any attachments from your computer. You should not retain, copy or
> use this
> > email or any attachments for any purpose, or disclose all or any part of
> the
> > contents to any person.  The LGL Group, Inc. and its subsidiaries
> reserve the
> > right to monitor all email communications through its networks.
> >
> >
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2