Hi Victor-
I don't understand your question. Must be the use of "discern". The pix Steve posted have identified/distinguished what appear to be voids within the laminate, so that would meet my interpretation of "discern".
I'd be concerned because the size range and variability of the voids suggests that you have a good chance of bridging conductors with a void somewhere. If that's the case, environmental stress and aging could create a current path.
Wayne
________________________________
From: [log in to unmask] [[log in to unmask]]
Sent: Monday, August 17, 2015 7:18 AM
To: [log in to unmask]; Wayne Thayer
Cc: [log in to unmask]
Subject: RE: [TN] Pros & Cons om laminate VOIDS
How can on call it an anomaly/defect if one is unable to discern the anomaly/defect.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: Friday, August 14, 2015 6:05 PM
To: [log in to unmask]
Subject: Re: [TN] Pros & Cons om laminate VOIDS
With this size range, I would be concerned. Nice sections!
Wayne
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, August 14, 2015 5:26 PM
To: [log in to unmask]
Subject: Re: [TN] Pros & Cons om laminate VOIDS
Hi Victor,
Here you go:
http://stevezeva.homestead.com/Laminate_voids.pdf
Steve
On Fri, Aug 14, 2015 at 12:23 PM, Victor Hernandez < [log in to unmask]> wrote:
> Fellow TechNetters:
>
> What are the Pros N Cons with LF laminate voids. Want to hear what
> the community thinks. I will upload photos to Steve Gregory shortly.
>
> Victor,
>
> Steve Gregory
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|