Richard,
Even if not, what is this indicative of? (I have seen it in the past)
Ed Popielarski
Engineering Manager
970 NE 21st Ct.
Oak Harbor, Wa. 98277
Ph: 360-675-1322
Fx: 206-624-0695
Cl: 949-581-6601
“It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design.”
https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Thursday, August 27, 2015 11:27 AM
To: [log in to unmask]
Subject: Re: [TN] ENIG coating durability
No problem. Send pictures of the pad surface after the parts were removed also, if you can. That can be very revealing.
One more question. On the bare PWBs not yet processed, are there pads that are a little bit more "orange" than gold in appearance?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Sullivan
Sent: Thursday, August 27, 2015 1:14 PM
To: [log in to unmask]
Subject: Re: [TN] ENIG coating durability
Sections and SEM are forthcoming.
I agree with both of you.
Richard: Apologies for my terminology. Yes... we assembled bare PCBs into CCAs and the problems appeared at this process.
Craig Sullivan
Manufacturing Engineer / IT Administrator
Phone: (607) 266-0480 x115
Fax: (607) 266-0482
Email: [log in to unmask]
Web: www.mplinc.com
MPL, Inc.
41 Dutch Mill Road | Ithaca | NY | 14850 P Please consider the environment before printing this e-mail.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman
Sent: Thursday, August 27, 2015 2:06 PM
To: [log in to unmask]
Subject: Re: [TN] ENIG coating durability
Hi Richard - good info. The issue Craig described could also just be oxidation of the nickel thus making solderability near zero and then the parts just "fall off".
Dave
On Thu, Aug 27, 2015 at 9:50 AM, Stadem, Richard D. < [log in to unmask]> wrote:
> I seldom see issues with ENIG-finished PWBs even after 5 years or
> longer, provided the ENIG finish was properly applied in the first
> place and the boards were stored properly during that time. ENIG, when
> done properly, is a very, very durable finish. The 4-5 uinches of gold
> will protect the underlying nickel very well, and that is what you
> actually solder to, not the gold.
> However, when problems such as those you are describing show up after
> soldering, it is a very strong indicator of Black Pad. If the ENIG is
> not plated properly and the immersion gold is not applied just right,
> after soldering the components you can send perfectly robust CCAs into
> the field, and in a few months the components can begin literally
> falling off the board. It sounds like what you are seeing is Black Pad.
> Just google up ENIG and Black Pad and you will see examples of the
> cratering and appearance of the pads, and compare them with the
> pictures of your own.
> Just about every time, the pictures are very similar.
> Quite often, much older ENIG PWBs from one vendor solder much better
> than those of another vendor that were fabricated and plated two weeks
> ago. This is due to the plating process controls (or lack thereof) at
> the fabricator, not the age of the plated PWB itself.
> Your email is a little bit confusing; when you state " PCBs just over
> a year old are showing signs of oxidation after processing, components
> can be flicked off with ease." Printed circuit boards (PCBs) are bare
> boards with no components assembled, whereas PCBs with components
> assembled are known as CCAs (Circuit Card Assemblies).
> If you mean that after the PCB is processed to solder components, and
> immediately after that the parts fall off, yes, that is a sign of one
> type of Black Pad, but it can also show up months later on assemblies
> that were perfectly robust immediately after soldering.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Sullivan
> Sent: Thursday, August 27, 2015 8:03 AM
> To: [log in to unmask]
> Subject: [TN] ENIG coating durability
>
> J-STD-003 and IPC-4552 basically state the ENIG should meet category 3
> (>6 months storage).
>
> My question is, what is the storage threshold for ENIG after the 6 months?
> 1 year, 2 years?
>
> What length of time should we conceivably expect to be able to store
> an ENIG board before seeing issues?
>
>
>
> Scenario: PCBs just over a year old are showing signs of oxidation
> after processing, components can be flicked off with ease. The Cu and
> Ni (if any
> left) on a PTH look horrendous after processing. Here's a kicker,
> these boards are date code 3414, but date code 3514 appears to be ok
> and solders fine, and date code 3114 shows a very low and random case
> of the oxidation/solderability issue.
>
>
>
> All PCBs stored in the same environment/manner
>
>
>
> Craig Sullivan
>
> Manufacturing Engineer / IT Administrator
>
> Phone: (607) 266-0480 x115
>
> Fax: (607) 266-0482
>
> Email: <mailto:[log in to unmask]> [log in to unmask]
>
> Web: <http://www.mplinc.com/> www.mplinc.com
>
>
>
> MPL, Inc.
>
> 41 Dutch Mill Road | Ithaca | NY | 14850
>
> P Please consider the environment before printing this e-mail.
>
>
>
> _____
>
> Confidentiality Notice:
> This e-mail contains privileged and confidential information which is
> the property of MPL Incorporated, intended only for the use of the
> intended recipient(s). Unauthorized use or disclosure of this
> information is prohibited. If you are not an intended recipient,
> please immediately notify MPL Incorporated and destroy any copies of
> this email. Receipt of this e-mail shall not be deemed a waiver by MPL
> Incorporated of any privilege or the confidential nature of the information.
>
> Export Control:
> This message is intended only for the addressee and may contain
> information that is company confidential or privileged. Any technical
> data in this message may be exported only in accordance with the U.S.
> International Traffic in Arms Regulations (22 CFR Parts 120-130) or
> the Export Administration Regulations (15 CFR Parts 730-774).
> Unauthorized use is strictly prohibited and may be unlawful. If you
> are not the intended recipient, or the person responsible for
> delivering to the intended recipient, you should not read, copy,
> disclose or otherwise use this message. If you have received this
> email in error, please delete it, and advise the sender immediately.
>
>
>
>
>
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|