TECHNET Archives

August 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Krug <[log in to unmask]>
Date:
Mon, 31 Aug 2015 13:46:46 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Subject:
From:
David Hillman <[log in to unmask]>
Message-ID:
In-Reply-To:
<EA4086ED2B7FA34CA6C1BA20A9A33992E4525914@ELKEX11>
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (92 lines)
Hi Dick - based on your information and the picture, I think what  you are
seeing is typical solder microstructure "texture". A cross section would be
definitive if you needed that level of confidence.

Dave

On Mon, Aug 31, 2015 at 1:28 PM, Richard Krug <[log in to unmask]> wrote:

> First, thanks for posting picture Steve.
>
> I'll try to answer all questions received thus far.
>         Solder is Sn63Pb37
>         Board is wave soldered.
>         Topside board temp before the wave ~115C
>         Leads of this component are solder dipped, alloy not specified,
> but SnPb.  Similar appearance on virtually all solder joints on the board.
>         This result was found on all boards of this work order, but not on
> other assemblies soldered on the same wave.
>         Flux coverage could be a cause, but dross is unlikely since not on
> other assemblies.
>         Flux is ORH.  Boards have been washed with saponified water.
>
> Thanks for the questions.
>
> Dick Krug, CSSBB, CSMTPE
> Lead Process Engineer
> Sparton Brooksville, LLC
> 30167 Power Line Road
> Brooksville, FL  34602-8299
> (352) 540-4012
> [log in to unmask]
>
>
> -----Original Message-----
> From: Guy Ramsey [mailto:[log in to unmask]]
> Sent: Monday, August 31, 2015 1:43 PM
> To: 'TechNet E-Mail Forum'; Richard Krug
> Subject: RE: [TN] Textured Solder?
>
> Might be past time to clean the wave guide. I have seen something like
> that when dross breaks off the inside of the guide and gets mixed in with
> the wave.
> I notice that three of the leads don't look like they wetted very well.
> Are you sure you have good flux coverage?
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Krug
> Sent: Monday, August 31, 2015 12:15 PM
> To: [log in to unmask]
> Subject: [TN] Textured Solder?
>
> I've got something I haven't seen before.  We wave soldered boards with
> Sn63Pb37 and found a "textured" surface after soldering.
> We seem to have good wetting, but it looks like we have "lumps"  under the
> solder surface.  The lumps are most visible where the solder is thin, but
> can also be found on thicker solder joints as well.
> The application is class 3.  We do monthly solder analysis on the pot so I
> don't think it is contamination in the solder.
> Any insights would be appreciated
>
> I know the picture will be stripped out of the message, but I'm copying
> Steve Gregory directly in hopes he can post the picture.
>
> Steve - Please post this picture to go with my question for the TechNet
> forum.  Thanks in advance.
>
> Dick Krug, CSSBB, CSMTPE
> Lead Process Engineer
> Sparton Brooksville, LLC
> 30167 Power Line Road
> Brooksville, FL  34602-8299
> (352) 540-4012
> [log in to unmask]
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2