TECHNET Archives

August 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum ([log in to unmask])" <[log in to unmask]>
Date:
Thu, 13 Aug 2015 11:34:47 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Gumpert, Ben" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Gumpert, Ben" <[log in to unmask]>
Parts/Attachments:
text/plain (12 lines)
TechNetters,

I've received several components recently that were plated with 'solderable nickel' and to my surprise they soldered just fine (using a ROL0 flux).
Anyone know what is going on to keep the nickel from oxidizing?

Ben

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2