TECHNET Archives

August 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 12 Aug 2015 12:39:26 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Vladimir Igoshev <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<008e01d0d434$3245af80$96d10e80$@com>
MIME-Version:
1.0
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (101 lines)
Interesting picture which creates more questions than give answers and definitely doesn't prove the point, at least to me.

Regards,

Vladimir

Sent from my BlackBerry 10 smartphone on the Rogers network.
  Original Message  
From: Guy Ramsey
Sent: Wednesday, August 12, 2015 12:26
To: [log in to unmask]
Reply To: [log in to unmask]
Subject: Re: [TN] immersion silver

http://blog.ipc.org/2009/04/20/gold-au-and-silver-ag-embrittlement-of-solder
-joints/


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
Sent: Tuesday, August 11, 2015 8:02 AM
To: [log in to unmask]
Subject: Re: [TN] immersion silver

Hi Guy,

With all due respect to Warner memory, silver IS NOT like gold and DOES NOT
cause embrittlement.

Therefore, from the reliability point of view it wouldn't matter what
thickness of IAg was on a board, as long as we ONLY talking about the amount
of Ag which would and up in the joints after re-flow.

Regards,

 Vladimir

Sent from my BlackBerry 10 smartphone on the Rogers network.
  Original Message
From: Guy Ramsey
Sent: Tuesday, August 11, 2015 07:37
To: [log in to unmask]
Reply To: [log in to unmask]
Subject: Re: [TN] immersion silver

If Werner were alive he would be reminding us that silver, like gold, is a
contaminate in tin solder. 
Early finishes, prior to 2005 or so, weren't good for multiple reflows. Some
presumed it was too thin.
I believe the problem was the durability of the organic additives that
retard oxidation of the silver.
Not perfect, but it is my preferred surface finish, but not too thick. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly
Sent: Monday, August 10, 2015 3:47 PM
To: [log in to unmask]
Subject: [TN] immersion silver

Hi All,
Why would someone choose thick immersion silver over thin? Are these
different chemistries? Regards Steve Kelly


Phone(O) (416) 750-8433
Phone (C) (416) 577-8433

If the recipient to whom this e-mail is sent has an NDA with PFC Flexible
Circuits Limited this e-mail is considered confidential and is subject to
any NDA agreements between the respective parties.

See PFC on "How its' Made" in Canada on July 7th at 8 p.m. on the Discovery
Channel


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2