Hi Ed! Phil and Jim are being way too nice and giving me too much credit!
The investigation they referenced was the NASA DoD Leadfree Soldering
project. It was a consortium effort with great work and analysis by a great
group of hard working people. Here is a link to the webpage on the project:
http://teerm.nasa.gov/nasa_dodleadfreeelectronics_proj2.htm
The same group of folks is working on a NASA DoD Phase 3 effort to take the
first two data sets and extend them to learn more about lead-free
soldering/processes.
Dave
On Thu, Jul 23, 2015 at 1:26 PM, Ed Popielarski <[log in to unmask]>
wrote:
> Dave Hillman was mentioned in a widely distributed article today!
>
> http://www.circuitinsight.com/programs/51504.html
>
> "I would like to point out that the consortium for the aerospace and
> military people, which our good friend, Dave Hillman has produced some of
> the best, most comprehensive test data... Dave, if we're wrong, please
> contact us. But the point is this is the only known published data
> comparing un-repaired boards with repaired boards that I know of."
>
> Ed Popielarski
> Engineering Manager
>
> [cid:[log in to unmask]]
> 970 NE 21st Ct.
> Oak Harbor, Wa. 98277
>
> Ph: 360-675-1322
> Fx: 206-624-0695
> Cl: 949-581-6601
>
>
>
> "It's one kind of victory to slay a beast, move a mountain, and
> cross a chasm, but it's another kind altogether to realize that the beast,
> the mountain, and the chasm were of your own design."
>
> https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|