TECHNET Archives

July 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 14 Jul 2015 08:15:18 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ong Seet Leng <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Ong Seet Leng <[log in to unmask]>
Parts/Attachments:
text/plain (14 lines)
Afternoon,

I had checked a bare printed wiring board and attached a photograph on one of the defect found. I would like to seek advice from you gurus' out there on what to call this defect? For the life of me, I can't find the definition of it. Appreciate if someone can guide me. Thanks in advance.

Regards,
Ong Seet Leng



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2