TECHNET Archives

June 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Wayne Thayer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Date:
Wed, 3 Jun 2015 20:51:08 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
And don't forget about the potential for nasty InCu intermetallics! If you
go with indium, nickel plate everything first.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: Wednesday, June 03, 2015 4:41 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Alloy SnIn - Working Environmental Conditions:
-100°C to +100°C

In/Sn solidus of 118C is almost certainly too low for 100C working
environment and there is not much benefit in ductility from this alloy at
the other end.
Probably Sn63 might cope in fact, but if you have large TEC mismatch, or
multiple cycles and other it depends stuff you might wish to look at an
In/Pb alloy. These are good for cryogenic apps so plenty in hand and you
have choice of MPs at other end of use scale. 
No benefit is without a cost though so you may have some surface finish
issues. To quote myself" it's never just the melting point" when it comes to
alloy choice. Discuss with your specialist supplier.

--
Regards 
 
Mike Fenner
BS&P
M: +44 [0] 7810 526 317
T: +44 [0] 1865 522 663

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ricardo Moncaglieri
Sent: Tuesday, June 02, 2015 10:18 PM
To: [log in to unmask]
Subject: [TN] Solder Alloy SnIn - Working Environmental Conditions: -100°C
to +100°C

Dear Colleagues,
Have to deploy a process and its qualification in order to perform
electrical connections which will be working under temperature variations in
the range of -100°C to +100°C (space application).
We are pointing to SnIn solder alloy.
We are just now starting  our investigation in our first steps.
Will be invaluable some advise as per your background so as directing me to
some std and/or paper about best applicable solder alloy and its
qualification method.
Being grateful in advance.
brgds, Ricardo Moncaglieri
 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2