TECHNET Archives

June 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Steve Gregory <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 30 Jun 2015 17:08:18 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Lehmicke, Michael" <[log in to unmask]>
Message-ID:
Subject:
From:
"Lehmicke, Michael" <[log in to unmask]>
Content-Transfer-Encoding:
base64
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Thanks Steve!


Mike Lehmicke
Project Engineer
Printed Circuit Products
Molex Incorporated
22 Empire Drive
St. Paul, MN 55103
651-846-7728
[log in to unmask]

[Logo_e-mail]<http://www.molex.com/>




From: Steve Gregory [mailto:[log in to unmask]]
Sent: Tuesday, June 30, 2015 11:30 AM
To: TechNet E-Mail Forum; Lehmicke, Michael
Subject: Re: [TN] Blue PCB material

Hi Mike,
Try these guys:

http://www.currentcomposites.com/html/electrical_grade_laminates.html
Steve

On Tue, Jun 30, 2015 at 10:13 AM, Lehmicke, Michael <[log in to unmask]<mailto:[log in to unmask]>> wrote:
Good morning;

I am looking for a source for blue PCB material. I will use copper clad laminates, but do not need the copper so I will take bare material also. I would like to get it in 18" x 24" sheets (or larger if necessary), looking for .026" thick.

Any ideas?

Thanks,

Mike


Mike Lehmicke
Project Engineer
Printed Circuit Products
Molex Incorporated
22 Empire Drive
St. Paul, MN 55103
651-846-7728<tel:651-846-7728>
[log in to unmask]<mailto:[log in to unmask]>

[Logo_e-mail]<http://www.molex.com/>





________________________________



CONFIDENTIALITY NOTICE: This message (including any attachments) may contain Molex confidential information, protected by law. If this message is confidential, forwarding it to individuals, other than those with a need to know, without the permission of the sender, is prohibited.

This message is also intended for a specific individual. If you are not the intended recipient, you should delete this message and are hereby notified that any disclosure, copying, or distribution of this message or taking of any action based upon it, is strictly prohibited.

English | Chinese | Japanese
www.molex.com/confidentiality.html<http://www.molex.com/confidentiality.html>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________


[http://fileserver1.kimco.net/PublicDocs/KDMsig200.png]

This email and any attachments are only for use by the intended recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.

________________________________



CONFIDENTIALITY NOTICE: This message (including any attachments) may contain Molex confidential information, protected by law. If this message is confidential, forwarding it to individuals, other than those with a need to know, without the permission of the sender, is prohibited.

This message is also intended for a specific individual. If you are not the intended recipient, you should delete this message and are hereby notified that any disclosure, copying, or distribution of this message or taking of any action based upon it, is strictly prohibited.

English | Chinese | Japanese
www.molex.com/confidentiality.html

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2