Steve,
Go to the Chip Quik web site, they make a lead free alloy, not sure of
the composition. $34 for 4.5 feet worth.
pat goodyear
On Tue, May 5, 2015 at 11:07 AM, Steve Gregory wrote:
> Hi All,
>
> Do any of you know if the Chip Quik Removal alloy (Tin 30%, Bismuth
> 56%,
> Indium 14%) works with lead-lead free solder?
>
> We have a board here that has to have some connectors reworked that
> are
> absolutely a bear to remove and I was wondering if it works with
> lead-free
> solder?
>
> Steve
>
> --
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential,
> proprietary or otherwise private information. Any unauthorized use,
> reproduction, dissemination, distribution or other disclosure of the
> contents of this e-mail or its attachments is strictly prohibited. If
> you have received this email in error, please notify the sender
> immediately and delete the original.
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
> service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|