Hi Lee - as part of the IPC JSTD 001 "State of the Industry Assessment" of
Conformal Coating Material & Application subcommittee activities, we looked
at a number of conformal coating thickness measurement
technologies/techniques since the test plan had 1,950 components to measure
representing 26 material/application sets. We found several very adequate
technologies for flat surfaces but as soon as you had a surface with any
level of topography, the ability to measure coating thickness became very
suspect. We settled on a very prescribed, rigid metallographic
cross-sectional technique that is working very well other than it is slow
and of course, destructive. I wish I had a better option for you but we
didn't have any success in finding an adequate nondestructive method for
nonflat surfaces. It is clearly a topic the industry needs and desires
better method for measurement option.
Dave Hillman
Rockwell Collins
[log in to unmask]
On Thu, May 7, 2015 at 2:49 AM, Lee Hitchens <[log in to unmask]>
wrote:
> Hi all
>
> I am being asked regularly now on options for measuring coating thickness
> on
> legs. I am trying to determine if there is actually a practical solution?
> Cost is less important compared to being a workable relatively quick
> process?
>
> One thing that could be an issue is many times its a silicone coating and
> this tends to be less than clear optically. Some systems need clear
> coatings
> to be successful.
>
> Has anyone had any success with this?
>
> Best Regards
>
> Dr Lee Hitchens
>
> SCH Technologies is a Division of SCH Services Limited
>
> Mob: +44 (0) 7862 25 33 21
>
> www.conformalcoating.co.uk <http://www.conformalcoating.co.uk/>
>
>
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|