Hi Dave,
In a past life this was used to rework through hole connectors on boards
that were approaching .300" thick and 40-layers, but that was using the
leaded version of the Solder Quik. The contamination of final solder joints
was minimized by re-filling the barrels with the final solder and then
extracting it to dilute the concentration of any residual solder that might
be left behind.
The issue that I have now is that we have a couple of boards that have
lifted connectors that need to be flush to the board. They're 42-pin Samtec
ESW-122-12-G-D connectors that run down the center of the board and,
there's SMT IC's all around them. I don't have an AirVac or anything like
it to rework the connectors. All we have is a heat gun and a solder
extractor. The board is constructed in such a way that it just sucks and
dissipates the heat away from the connectors. We have a very good rework
lady here and she is just pulling her hair out trying to rework these
things. She had to remove a smaller connector and wound-up destroying the
connector and pulling it out pin by pin. That connector didn't have all the
SMT around it that the 42-pin ones do, so I'm trying to help her rework
these boards without pulling a barrel or delaminating the board.
It's only been a few times that I've run across a .062" board that
dissipates heat like this...it's really weird.
Steve
On Tue, May 5, 2015 at 2:54 PM, David Hillman <
[log in to unmask]> wrote:
> Hi Steve - assuming you are using SAC305 solder, then any element(s) you
> "add" to the SAC305 solder joints that has a lower melting temperature will
> allow you to remove the connectors at a lower temperature. Since indium
> melts at 157C, you would lower the melting point of SAC305 to something
> below 217C depending on what the final solder composition ends up being.
> And depending on the alloy phase diagram, you could end up being even lower
> if specific alloy combinations are formed. The bigger issue is that if you
> don't get all of the "new" solder composition off the pads or the connector
> (if you planned on reusing it) as part of your rework process, then you
> will have unknown solder joint integrity which may or may not be
> appropriate for the product use environment. Food for thought.
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
> On Tue, May 5, 2015 at 1:07 PM, Steve Gregory <[log in to unmask]> wrote:
>
>> Hi All,
>>
>> Do any of you know if the Chip Quik Removal alloy (Tin 30%, Bismuth 56%,
>> Indium 14%) works with lead-lead free solder?
>>
>> We have a board here that has to have some connectors reworked that are
>> absolutely a bear to remove and I was wondering if it works with lead-free
>> solder?
>>
>> Steve
>>
>> --
>>
>>
>> This email and any attachments are only for use by the intended
>> recipient(s) and may contain legally privileged, confidential, proprietary
>> or otherwise private information. Any unauthorized use, reproduction,
>> dissemination, distribution or other disclosure of the contents of this
>> e-mail or its attachments is strictly prohibited. If you have received
>> this
>> email in error, please notify the sender immediately and delete the
>> original.
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>
>
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary
or otherwise private information. Any unauthorized use, reproduction,
dissemination, distribution or other disclosure of the contents of this
e-mail or its attachments is strictly prohibited. If you have received this
email in error, please notify the sender immediately and delete the
original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|