Careful, you may not be allowed to use it without customer approval.
You may be required to qualify such a rework process before you jump in and start changing alloys.
Introduction of other alloys does present possible reliability issues with the resultant solder joints.
If your assembly drawing states to solder with Sn63/37 or SAC305 that meets the requirements of J-STD-003 or -004 or whatever, you cannot give your customer anything except that.
And do not think that if you remove a part with it, then wick off all the solder, and solder the new part on with the required solder, you are OK. The IMC formed may not actually meet the requirements.
Just keep that in mind before you start "experimenting" on production CCAs.
Dean
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, May 05, 2015 1:08 PM
To: [log in to unmask]
Subject: [TN] Chip Quik Removal Alloy
Hi All,
Do any of you know if the Chip Quik Removal alloy (Tin 30%, Bismuth 56%, Indium 14%) works with lead-lead free solder?
We have a board here that has to have some connectors reworked that are absolutely a bear to remove and I was wondering if it works with lead-free solder?
Steve
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|