Hi Steve
I used to make these. Bake them overnight >12 hours at 80C. That should do the trick. Let me know if it doesn’t.
I assume these will be a silicone “rubber”. Who is your supplier - Kinarney Rubber in New England? If not, give them a call.
Graham Naisbitt
> On 14 Apr 2015, at 17:25, Steve Gregory <[log in to unmask]> wrote:
>
> Thanks Doug! So is there anything you can do, like wash them in alcohol or
> something?
>
> Steve
>
> On Tue, Apr 14, 2015 at 10:23 AM, Douglas Pauls <
> [log in to unmask]> wrote:
>
>> Steve,
>> In my experience they do. We sometimes see the same thing, whether molded
>> rubber or molded vinyl.
>>
>>
>> Doug Pauls
>> Principal Materials and Process Engineer
>> Rockwell Collins
>>
>> On Tue, Apr 14, 2015 at 11:21 AM, Steve Gregory <[log in to unmask]>
>> wrote:
>>
>>> Hi All,
>>>
>>> Just got some black ESD rubber masking boots for some blade terminals for
>>> a
>>> board that we dip in Humiseal 1A33, and noticed that there is shadowing
>>> around the base of the terminals like something was repelling the coating
>>> away from them, maybe some sort of mold release compound? Tried dipping
>>> without the boots and we don't see the shadow. I got the boots to keep the
>>> coating from getting on the terminals so that we weren't sitting there
>>> with
>>> a conformal coat removal pen cleaning the terminals up after we dipped the
>>> boards.
>>>
>>> I called the manufacturer of the boots and asked about the issue, and he
>>> said they would get back to me. Haven't heard anything yet. I'll try to
>>> get
>>> a picture that shows you what I'm talking about...
>>>
>>> Steve
>>>
>>> --
>>>
>>>
>>> This email and any attachments are only for use by the intended
>>> recipient(s) and may contain legally privileged, confidential, proprietary
>>> or otherwise private information. Any unauthorized use, reproduction,
>>> dissemination, distribution or other disclosure of the contents of this
>>> e-mail or its attachments is strictly prohibited. If you have received
>>> this
>>> email in error, please notify the sender immediately and delete the
>>> original.
>>>
>>>
>>> ______________________________________________________________________
>>> This email has been scanned by the Symantec Email Security.cloud service.
>>> For more information please contact helpdesk at x2960 or [log in to unmask]
>>> ______________________________________________________________________
>>>
>>
>>
>
> --
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential, proprietary
> or otherwise private information. Any unauthorized use, reproduction,
> dissemination, distribution or other disclosure of the contents of this
> e-mail or its attachments is strictly prohibited. If you have received this
> email in error, please notify the sender immediately and delete the
> original.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|