TECHNET Archives

April 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"lduso - Diamond-MT.com" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, lduso - Diamond-MT.com
Date:
Wed, 15 Apr 2015 16:52:30 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (48 lines)
Doug

Have you checked out Paul N. Gardner company? Website is Gardco.com They
have a huge selection including their own brand. Plus their technical guys
are great.

Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com

On Wed, Apr 15, 2015 at 4:23 PM, Douglas Pauls <
[log in to unmask]> wrote:

> Good afternoon all,
>
> I have a silly question.  We conformally coat using  a common solvent based
> acrylic coating.  One process control method is to periodically measure
> coating viscosity using a Zahn #2 cup, which works well for this particular
> coating that has about a 55-60 second flow.  I am finding that when this
> coating is thinned down for spray, the times are down in the 15-18 second
> range and the variation is increasing.
>
> So, my question - is there a style of viscosity dip cup, e.g. Ford, DIN,
> etc., that is more amenable to thin viscosity coatings?  It is understood
> that a precision instrument like a Brookfield viscometer would be
> preferrable, but production is NOT going to let me get a few dozen of them.
>
> Thanks.
>
> Doug Pauls
> Principal Materials and Process Engineer
> Rockwell Collins
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2