Good Afternoon Victor et al,
I'm unsure if you are talking about copper bond wires between the die and the lead frame or something else...
Assuming you are talking the die to lead frame, then there are a number of studies showing that that a number of changes are required to maintain reliability due to differences in the inter-metallic area and the susceptibility of that area to various chemicals, such as Cl.
The change from gold bond wire to copper bond wire is definitely not simple & if a supplier is proposing it be sure to make sure they have done their homework or you may have reliability issues.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Tuesday, April 14, 2015 9:01 AM
To: [log in to unmask]
Subject: [TN] Copper Wire Bonds
Fellow TechNetters:
What is the story behind Copper Wire Bonds. I have heard of them but now I have witness one. Any details out there on this technology? I will have to search archives.
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
**********************
** LEGAL DISCLAIMER **
**********************
This E-mail message and any attachments may contain
legally privileged, confidential or proprietary
information. If you are not the intended recipient(s),
or the employee or agent responsible for delivery of
this message to the intended recipient(s), you are
hereby notified that any dissemination, distribution
or copying of this E-mail message is strictly
prohibited. If you have received this message in
error, please immediately notify the sender and
delete this E-mail message from your computer.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|