3m products work well. We use the standard green masking tape everyday.
Shercon products work well also, that's where all our dots come from. Some
tapes do not work well with some Acrylics though. Seems to depend on the
thinners used in the acrylics. It will cause de-wetting.
Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com
On Thu, Apr 2, 2015 at 11:14 AM, Ed Popielarski <[log in to unmask]>
wrote:
> This works well:
> http://www.matweb.com/search/datasheettext.aspx?matguid=e7d952bc8bda462b9c3fe6a2db28bed3
>
> Ed Popielarski
> Engineering Manager
>
>
> 970 NE 21st Ct.
> Oak Harbor, Wa. 98277
>
> Ph: 360-675-1322
> Fx: 206-624-0695
> Cl: 949-581-6601
>
>
>
> “It's one kind of victory to slay a beast, move a mountain, and
> cross a chasm, but it's another kind altogether to realize that the beast,
> the mountain, and the chasm were of your own design.”
>
> https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
> Sent: Thursday, April 02, 2015 8:08 AM
> To: [log in to unmask]
> Subject: [TN] Masking tape recommendations for Acrylic conformal coating...
>
> Morning All,
>
> I know this has been posted before, and for some reason I can't search the
> archives.
>
> We're starting to do acrylic coating on some assemblies here, and I was
> looking for some recommendations for masking tape that doesn't leave
> residues.
>
> Can anybody give some recommendations?
>
> Steve
>
> --
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential, proprietary
> or otherwise private information. Any unauthorized use, reproduction,
> dissemination, distribution or other disclosure of the contents of this
> e-mail or its attachments is strictly prohibited. If you have received this
> email in error, please notify the sender immediately and delete the
> original.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|