Steve
Just about all the boots we have used have had some sort of release agent
but I have never had any that caused de-wetting. Especially with 1A33. That
material wets better then most other coatings. i have had some that left a
residue on the tab that glowed under the UV light. The customer swore it
was coating.
We started using tab boots from Caplugs.com . Minimal residue. no dewetting
that we have seen from all the coatings we have used.
Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com
On Tue, Apr 14, 2015 at 12:21 PM, Steve Gregory <[log in to unmask]> wrote:
> Hi All,
>
> Just got some black ESD rubber masking boots for some blade terminals for a
> board that we dip in Humiseal 1A33, and noticed that there is shadowing
> around the base of the terminals like something was repelling the coating
> away from them, maybe some sort of mold release compound? Tried dipping
> without the boots and we don't see the shadow. I got the boots to keep the
> coating from getting on the terminals so that we weren't sitting there with
> a conformal coat removal pen cleaning the terminals up after we dipped the
> boards.
>
> I called the manufacturer of the boots and asked about the issue, and he
> said they would get back to me. Haven't heard anything yet. I'll try to get
> a picture that shows you what I'm talking about...
>
> Steve
>
> --
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential, proprietary
> or otherwise private information. Any unauthorized use, reproduction,
> dissemination, distribution or other disclosure of the contents of this
> e-mail or its attachments is strictly prohibited. If you have received this
> email in error, please notify the sender immediately and delete the
> original.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|