try wire solder Sn05Pb92.5Ag2.5 it is a eutectic melting at 280°C
Works well from our experience.
Roger Mack P.Eng.
Manufacturing Specialist
Parker Hannifin Canada
Electronic Controls Division
1305 Clarence Avenue
Winnipeg, MB R3T 1T4 Canada
direct 204 453 3339 x7373
[log in to unmask]
www.parker.com/ecd
From: David Hillman <[log in to unmask]>
To: <[log in to unmask]>
Date: 2015-04-01 09:57 AM
Subject: Re: [TN] HIGH Temperature Solder
Sent by: TechNet <[log in to unmask]>
Hi Jeff - here are a couple of other choices:
10Sn88Pb2Ag
1Sn97.5Pb1.5Ag
97Pb3Ag
Nothing wrong with you 90Pb10Sn either. Make sure you select a flux core
that has good thermal stability as your soldering temperatures are much
hotter than what you deal with when using the Sn63Pb37 alloy. Also
consider
what the cleaning (or not cleaning) issues you may have to deal with.
Dave Hillman
Rockwell Collins
[log in to unmask]
On Wed, Apr 1, 2015 at 9:20 AM, McGlaughlin, Jeffrey A <
[log in to unmask]> wrote:
> I need to spec a high temperature wire solder for hand soldering. I need
> to have a solidus of greater than 250 degrees C. Is 90Pb10Sn my
best/only
> choice or is there something else I should look at?
>
> Jeffrey McGlaughlin, C.I.D.
> Engineering Designer
> Avionics Systems & Tech Refersh
> Office: 614.424.7582| Fax: 614.458.7582
> [log in to unmask]<mailto:[log in to unmask]>
>
> Battelle
> 505 King Avenue
> Columbus Ohio 43201-2693
> http://www.battelle.org<http://www.battelle.org/>
>
> Connect with Battelle
> Facebook<http://www.facebook.com/battelle> | LinkedIn<
> http://www.linkedin.com/company/battelle>
> Twitter<http://www.twitter.com/Battelle> | YouTube<
> http://www.youtube.com/user/battelleinnovations>
>
> This message is intended only for the use of the individual or entity to
> which it is addressed, and may contain information that is privileged,
> confidential and/or otherwise exempt from disclosure under applicable
law.
> If the reader of this message is not the intended recipient or the
employee
> or agent responsible for delivering the message to the intended
recipient,
> any disclosure, dissemination, distribution, copying or other use of
this
> communication or its substance is prohibited. If you have received this
> communication in error, please return to the sender and delete from your
> computer system.
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or
[log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|