Good Morning TechNet!
Has anyone experienced or documented any examples (photos, DPA reports, chemical analysis, etc.) of the type of dielectric staining referenced in the Rogers application note below? This concern applies to composite PTFE laminates with a large volume fraction (>50%) of ceramic filler particles.
http://www.rogerscorp.com/documents/643/acm/The-Prevention-and-Removal-of-Absorbed-Chemicals-in-Ceramic-Filled-PTFE-Composites.pdf
Key Excerpts:
The material's high filler loading also contributes to approximately 5 volume percent porosity.
Low surface tension liquids such as organic solvents and surfactant laden aqueous solutions can penetrate the pores.
Failure to adequately rinse these laminates following exposure to process chemicals can sometimes result
in dielectric staining or increased dielectric loss.
I think we may be dealing with this issue and would appreciate any relevant details you may wish to share (specific dielectric materials, photos, DPA reports, chemical analyses, dispositions/resolutions, etc.)
Thank you!
John Nieznanski
________________________________
This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of Exelis Inc. The recipient should check this e-mail and any attachments for the presence of viruses. Exelis Inc. accepts no liability for any damage caused by any virus transmitted by this e-mail.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|