what is the seal material? the substrate surface finishing? (especially
the lid surface finishing). If you use polymeric material as a seal, your
fine leak test doesn't mean anything - He got absorbed in the polymer...
is it glass or metal seal? what kind? please don't drop a satellite on
my head on Fri the 13.
jk
> Drew,
>
> Thanks for the feedback, and it is good to hear that someone has seen this
> defect before with a cerdip. I was wondering if this type of problem might
> be more prevalent with the cerdips.
>
> Howard A. Watson
>
>
> -----Original Message-----
> From: [log in to unmask] [mailto:[log in to unmask]]
> Sent: Friday, March 13, 2015 8:57 AM
> To: [log in to unmask]; Watson, Howard August
> Cc: [log in to unmask]
> Subject: RE: Mechanical failure of 8-pin Cerdip
>
> Howard,
>
> Not common but it does happen. I have witnessed this once. When I was
> working at Fisher Controls International. This was in the pre ICT days.
> Each assembly type had a custom made test box designed and built for it.
> One of the test department folks called us out to see this. He had a
> completed assembly on the test box. The assembly was fully functional,
> passed all set up and test process. When he had finished test he noticed
> a fourteen pin Cerdip missing it's lid. Electrically sound. We joked
> about shipping it that way but of course off to repair it went. Cerdips
> can fail at the glue line if impacted hard or if the bond was compromised
> in some fashion when it was made. As long as it is very rare all you can
> do is scrap the bad part or tube of parts if your uncomfortable with the
> risk on the balance of parts in the tube.
>
> Drew Meyer
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Watson, Howard August
> Sent: Friday, March 13, 2015 9:36 AM
> To: [log in to unmask]
> Subject: [TN] Mechanical failure of 8-pin Cerdip
>
> Hello TechNet,
>
> I have an IC Op Amp that was found in stock with the lid separated. The
> stock room discovered this while kitting components, so this part was
> minimally handled. It was stored in the original IC tube. Collectively, we
> have never seen an occurrence of something like this, and I wonder if any
> of you have experienced this before. The explanation I got from the
> manufacturer is that it is most likely a packing and/or handling problem
> and that if there is too much slack in the tubes, the parts colliding
> together could cause the lid to pop off. Wouldn't the seal material be
> more robust than to allow the lid to pop off? My concern is that we have
> 120 of these all from one lot, and if there was a processing problem, then
> maybe I have some other poorly bonded lids that may separate. Do you think
> my concern is valid, or is this a one-off rare handling caused defect?
> These are space grade parts.
>
> Thanks to Steve, a couple pictures are posted on the links below. I don't
> know what could be determined from the first picture, other than yes, the
> lid definitely popped off! The second picture shows another IC with a lid
> slightly skewed, but within tolerance I believe. Thanks in advance for any
> suggestions you can offer.
>
> http://stevezeva.homestead.com/RH1078MJ8-1.jpg
> http://stevezeva.homestead.com/RH1078MJ8-2.jpg
>
> Howard A. Watson
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|